Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 738 MPa @Temperature 82.2 °C |
107000 psi @Temperature 180 °F |
0° Direction, Dry; ASTM D3039 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Tensile Strength, Yield | 741 MPa @Strain 0.200 %, Thickness 1.45 mm |
107000 psi @Strain 0.200 %, Thickness 0.0571 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 735 MPa @Diameter 12.7 mm |
107000 psi @Diameter 0.500 in |
Welded then age-hardened; 0.2% offset |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | >= 740 MPa @Thickness >=65.0 mm |
>= 107000 psi @Thickness >=2.56 in |
|
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Tensile Strength, Yield | >= 740 MPa @Thickness >=65.0 mm |
>= 107000 psi @Thickness >=2.56 in |
|
ThyssenKrupp N-A-XTRA® M 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Tensile Strength, Yield | 738 MPa @Temperature 25.0 °C |
107000 psi @Temperature 77.0 °F |
Quasi-Isotropic 25/50/25, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |