Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 10700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 73.5 MPa

@Thickness 3.20 mm
10700 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Bhansali Engineering Santron IMS 2007LF SAN Resin
High Rigidity Clear SANInformation provided by Bhansali
Tensile Strength, Yield 73.5 MPa

@Thickness 3.20 mm
10700 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Bhansali Engineering Santron IMS 2007LF SAN Resin
High Rigidity Clear SANInformation provided by Bhansali