Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
Type I, 50 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 73.5 MPa @Thickness 3.20 mm |
10700 psi @Thickness 0.126 in |
Type I, 50 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |