Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 689 MPa @Thickness 15.9 - 114 mm |
>= 100000 psi @Thickness 0.625 - 4.50 in |
|
Niagara LaSalle CPO® Cold Finished Steel Bar CPO® chrome plated steel bars and tubes are manufactured to meet the specific needs for piston rod material in hydraulic and pneumatic cylinders. They are readily available in standard and custom s.. |
|||
Tensile Strength, Yield | >= 689 MPa @Thickness 15.9 - 114 mm |
>= 100000 psi @Thickness 0.625 - 4.50 in |
|
Niagara LaSalle IHCP® Cold Finished Steel Bar IHCP® steel bars and tubes are manufactured to meet the specific needs for piston rod material in hydraulic and pneumatic cylinders. They are readily available in standard and custom sizes, chemist.. |
|||
Tensile Strength, Yield | 689 MPa @Temperature 23.9 °C |
100000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Strength, Yield | >= 689 MPa @Strain 0.200 %, Thickness 0.254 - 0.635 mm |
>= 100000 psi @Strain 0.200 %, Thickness 0.0100 - 0.0250 in |
ASTM E-8 |
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength, Yield | >= 689 MPa @Strain 0.200 %, Thickness 0.635 - 1.52 mm |
>= 100000 psi @Strain 0.200 %, Thickness 0.0250 - 0.0600 in |
ASTM E-8 |
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength, Yield | >= 689 MPa @Strain 0.200 %, Thickness 1.52 - 2.29 mm |
>= 100000 psi @Strain 0.200 %, Thickness 0.0600 - 0.0900 in |
ASTM E-8 |
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength, Yield | >= 689 MPa @Strain 0.200 %, Thickness 2.29 - 4.75 mm |
>= 100000 psi @Strain 0.200 %, Thickness 0.0900 - 0.187 in |
ASTM E-8 |
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength, Yield | >= 689 MPa @Strain 0.200 %, Thickness 4.762 - 12.7 mm |
>= 100000 psi @Strain 0.200 %, Thickness 0.1875 - 0.500 in |
ASTM E-8 |
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength, Yield | >= 689 MPa @Diameter 3.17 - 22.2 mm, Strain 0.200 % |
>= 100000 psi @Diameter 0.125 - 0.875 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Molybdenum Alloy PBT, Bar Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg.. |
|||
Tensile Strength, Yield | >= 689 MPa @Diameter 3.17 - 22.2 mm, Strain 0.200 % |
>= 100000 psi @Diameter 0.125 - 0.875 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma.. |
|||
Tensile Strength, Yield | 690 MPa @Strain 0.200 %, Temperature 20.0 °C |
100000 psi @Strain 0.200 %, Temperature 68.0 °F |
Transverse |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 690 MPa @Strain 0.200 %, Temperature 25.0 °C |
100000 psi @Strain 0.200 %, Temperature 77.0 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |