Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 143 x 10-8 mm³/N-M | 71.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant. |