Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 142 x 10-8 mm³/N-M | 70.6 x 10-10 in³-min/ft-lb-hr | at 5000 psi - fpm PV; ASTM D3702 |
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |