Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 120 x 10-8 mm³/N-M @Pressure 1.75 MPa |
59.6 x 10-10 in³-min/ft-lb-hr @Pressure 254 psi |
31.4m/min |
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled) This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E.. |
|||
K (wear) Factor | 120 x 10-8 mm³/N-M | 59.6 x 10-10 in³-min/ft-lb-hr | |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
K (wear) Factor | 120 x 10-8 mm³/N-M | 59.6 x 10-10 in³-min/ft-lb-hr | |
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity an.. |