Polymer Property : K (wear) Factor = 120 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 120 x 10-8 mm³/N-M

@Pressure 1.75 MPa
59.6 x 10-10 in³-min/ft-lb-hr

@Pressure 254 psi
31.4m/min
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled)
This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E..
K (wear) Factor 120 x 10-8 mm³/N-M
59.6 x 10-10 in³-min/ft-lb-hr
Polikim KESTOIL® Polyamide 6 + Lubricant
Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio..
K (wear) Factor 120 x 10-8 mm³/N-M
59.6 x 10-10 in³-min/ft-lb-hr
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled
Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity an..