Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 103 x 10-8 mm³/N-M | 51.0 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Lubricomp® OFL-4536 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
K (wear) Factor | 103 x 10-8 mm³/N-M | 51.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Glass Fiber, Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SA.. |
|||
K (wear) Factor | 103 x 10-8 mm³/N-M | 51.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Silicone, PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.This data was supplied by SA.. |
|||
K (wear) Factor | 103 x 10-8 mm³/N-M | 51.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
K (wear) Factor | 103 x 10-8 mm³/N-M | 51.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |