Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 3.00 - 5040 x 10-8 mm³/N-M | 1.49 - 2500 x 10-10 in³-min/ft-lb-hr | Average value: 1920 x 10<sup>-8</sup> mm³/N-M Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
K (wear) Factor | 10.0 - 5040 x 10-8 mm³/N-M | 4.96 - 2500 x 10-10 in³-min/ft-lb-hr | Average value: 4080 x 10<sup>-8</sup> mm³/N-M Grade Count:18 |