Polymer Property : K (wear) Factor = 2500 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 3.00 - 5040 x 10-8 mm³/N-M
1.49 - 2500 x 10-10 in³-min/ft-lb-hr
Average value: 1920 x 10<sup>-8</sup> mm³/N-M Grade Count:7
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
K (wear) Factor 10.0 - 5040 x 10-8 mm³/N-M
4.96 - 2500 x 10-10 in³-min/ft-lb-hr
Average value: 4080 x 10<sup>-8</sup> mm³/N-M Grade Count:18
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..