Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 500 x 10-8 mm³/N-M @Pressure 1.75 MPa |
248 x 10-10 in³-min/ft-lb-hr @Pressure 254 psi |
31.4m/min |
Nylacast PA6C Cast Nylon 6 Natural PA6 is the base to the other grades of material offered by Nylacast. It is available in Natural (off white) or Black colour. It is made by ionic polymerisation of e-caprolactam under anhydri.. |
|||
K (wear) Factor | 500 x 10-8 mm³/N-M | 248 x 10-10 in³-min/ft-lb-hr | |
Polikim KESTAMID® PA6G Polyamide 6 Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical.. |
|||
K (wear) Factor | 500 x 10-8 mm³/N-M @Pressure 1.75 MPa |
248 x 10-10 in³-min/ft-lb-hr @Pressure 254 psi |
31.4 m/min |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
K (wear) Factor | 500 x 10-8 mm³/N-M | 248 x 10-10 in³-min/ft-lb-hr | |
Polikim KESTAMID® HS Polyamide 6, Heat Resistant Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with .. |