Polymer Property : K (wear) Factor = 3.00 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 4.03 - 6.04 x 10-8 mm³/N-M
2.00 - 3.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT
LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.