Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 52.4 x 10-8 mm³/N-M | 26.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
K (wear) Factor | 52.4 x 10-8 mm³/N-M | 26.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
K (wear) Factor | 52.4 x 10-8 mm³/N-M | 26.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
K (wear) Factor | 52.4 x 10-8 mm³/N-M | 26.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |