Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 449 x 10-8 mm³/N-M | 223 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubriloy DF202 PC LNP LUBRILOY* DF202 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied b.. |
|||
K (wear) Factor | 449 x 10-8 mm³/N-M | 223 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY DF202P PC LNP LUBRILOY* DF202P is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Exceptional Processing. |