Material Notes:
LNP LUBRILOY* DF202 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
ASTM D 638
Elongation at Break 4.0 %
4.0 %
ASTM D 638
Flexural Strength 132 MPa
19100 psi
ASTM D 790
Flexural Modulus 4.06 GPa
589 ksi
ASTM D 790
Izod Impact, Notched 1.76 J/cm

@Temperature 23.0 °C
3.30 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 7.47 J/cm

@Temperature 23.0 °C
14.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D 3702 Modified
Coefficient of Friction, Static 0.30
0.30
ASTM D 3702 Modified
K (wear) Factor 449 x 10-8 mm³/N-M
223 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified