Mechanical Properties Metric English Comments
K (wear) Factor 183 x 10-8 mm³/N-M
91.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC
LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 183 x 10-8 mm³/N-M
91.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific)
LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 183 x 10-8 mm³/N-M
91.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC
LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing 20% Milled Glass, 15% PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 183 x 10-8 mm³/N-M
91.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC (Asia Pacific)
LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.