Mechanical Properties Metric English Comments
K (wear) Factor 179 x 10-8 mm³/N-M
89.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC
LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant.
K (wear) Factor 179 x 10-8 mm³/N-M
89.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
K (wear) Factor 179 x 10-8 mm³/N-M
89.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..