Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 161 x 10-8 mm³/N-M | 80.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
K (wear) Factor | 161 x 10-8 mm³/N-M | 80.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
K (wear) Factor | 161 x 10-8 mm³/N-M | 80.0 x 10-10 in³-min/ft-lb-hr | Thrust washer at 2000 PV |
Techmer ES Plaslube® J-3/30/TF/15 Nylon 6, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
K (wear) Factor | 161 x 10-8 mm³/N-M | 80.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66 LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
K (wear) Factor | 161 x 10-8 mm³/N-M | 80.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
K (wear) Factor | 161 x 10-8 mm³/N-M | 80.0 x 10-10 in³-min/ft-lb-hr | |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |