Polymer Property : K (wear) Factor = 80.0 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 161 x 10-8 mm³/N-M
80.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)
K (wear) Factor 161 x 10-8 mm³/N-M
80.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific)
LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec..
K (wear) Factor 161 x 10-8 mm³/N-M
80.0 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Techmer ES Plaslube® J-3/30/TF/15 Nylon 6, 30% GFR, 15% PTFE
Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha..
K (wear) Factor 161 x 10-8 mm³/N-M
80.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66
LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber.
K (wear) Factor 161 x 10-8 mm³/N-M
80.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66
LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber.
K (wear) Factor 161 x 10-8 mm³/N-M
80.0 x 10-10 in³-min/ft-lb-hr
TriStar TriSteel AT Metal Backed PTFE Bearing System
Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li..