Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 310 x 10-8 mm³/N-M | 154 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP EFL24P PEI LNP* LUBRICOMP* EFL24P is a compound based on Polyetherimide resin containing 20% Glass Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Exceptional Processing. |