Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 292 x 10-8 mm³/N-M | 145 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |