Polymer Property : K (wear) Factor = 142 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 286 x 10-8 mm³/N-M
142 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66
LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant.