Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 127 - 179 x 10-8 mm³/N-M | 63.0 - 89.0 x 10-10 in³-min/ft-lb-hr | Average value: 148 x 10<sup>-8</sup> mm³/N-M Grade Count:5 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 (Asia Pacific) LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant.. |
|||
K (wear) Factor | 127 x 10-8 mm³/N-M | 63.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific) LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |