Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer containing Graphite. Added features include : Internally Lubricated. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66 LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific) LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 (Asia Pacific) LNP* THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
K (wear) Factor | 207 x 10-8 mm³/N-M | 103 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 LNP THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas.. |