Polymer Property : K (wear) Factor = 0.894 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 1.80 x 10-8 mm³/N-M
0.894 x 10-10 in³-min/ft-lb-hr
LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled
Self-lubricating product based on Polyoxymethylene (POM). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
K (wear) Factor 1.80 - 399 x 10-8 mm³/N-M
0.894 - 198 x 10-10 in³-min/ft-lb-hr
Average value: 99.3 x 10<sup>-8</sup> mm³/N-M Grade Count:10
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..