Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 427 MPa | 62000 psi | ASTM D638 |
ExxonMobil LLDPE LL 5001.09 Linear Low Density Polyethylene Resin Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending .. |