Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LLDPE LL 5001.09 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 5001.09 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending with pigments, slip and antiblock additives.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: No Thermal Stabilizer: YesApplications: Masterbatch Base ResinInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50

@Time 15.0 sec
50

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
ASTM D638
Tensile Strength, Yield 14.5 MPa
2100 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Modulus, 1% Secant 427 MPa
62000 psi
ASTM D638
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 252 °C
<= 486 °F
Peak Melting Point; ExxonMobil method
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Copyright © lookpolymers.com All Rights Reserved