Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1790 MPa | 260000 psi | ASTM D790A |
Ineos H65C-00 Polypropylene Homopolymer This is a high melt flow clarified and lightly lubricated homopolymer designed for high-speed injection molding. It exhibits excellent see-through clarity and meets the requirements of the U.S. Foo.. |