Material Notes:
This is a high melt flow clarified and lightly lubricated homopolymer designed for high-speed injection molding. It exhibits excellent see-through clarity and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer productsAudio-video media packaging formats (DVD and CD cases)Thin-wall injection molding, dairy/dessert rigid packaging (TWIM)HousewaresBenefitsExcellent clarityFast cyclingLow blooming with good mold releaseExcellent performance in TWIM parts and food containersInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 65 g/10 min

@Load 2.16 kg,
Temperature 230 °C
65 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 39.3 MPa

@Temperature 23.0 °C
5700 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus, 1% Secant 1790 MPa
260000 psi
ASTM D790A
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
ASTM D648
Optical Properties Metric English Comments
Haze 15 %
15 %
50-mil plaque, % Diffuse Transmittance; ASTM D1003