Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1340 MPa | 194000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |
|||
Flexural Modulus, 1% Secant | 1340 MPa | 194000 psi | ASTM D790A |
Dow C700-35 Polypropylene Impact Copolymer Resin OverviewHigh stiffnessGood mold fillabilityComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35 Polypropylene Resin is intended for use in injection molding processes where medium .. |
|||
Flexural Modulus, 1% Secant | 1340 MPa | 194000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |