Flexural Modulus, 1% Secant 1210 MPa
176000 psi
0.5 in/min; ASTM D790B
ExxonMobil PP7505KNE2 Polypropylene Homopolymer
Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced ..