Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1210 MPa | 175000 psi | 0.05 in/min; ASTM-D790 |
CTC X-PRO CTC PP1020 Polypropylene Homopolymer X-PRO PP 1020 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Flexural Modulus, 1% Secant | 1210 MPa | 175000 psi | 0.05 in/min; ASTM-D790 |
CTC X-PRO CTC PP1035 Polypropylene Homopolymer X-PRO PP 1035 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Flexural Modulus, 1% Secant | 1210 MPa | 175000 psi | 0.05 in/min; ASTM-D790 |
CTC X-PRO CTC PP1050 Polypropylene Homopolymer X-PRO PP 1050 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Flexural Modulus, 1% Secant | 1210 MPa | 175000 psi | 0.05 in/min; ASTM-D790 |
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Flexural Modulus, 1% Secant | 1210 MPa | 176000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP7505KNE2 Polypropylene Homopolymer Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced .. |
|||
Flexural Modulus, 1% Secant | 1210 MPa | 175000 psi | ASTM D790 |
Entec Hypro™ PP-CP20/10 Impact Copolymer, 20 Melt Flow This product is intended for general purpose injection molding applications including flooring, automotive, appliance, lawn and garden and industrial application.Information provided by Entec |
|||
Flexural Modulus, 1% Secant | 1210 MPa | 175000 psi | ASTM D790A |
Dow C702-20NA Polypropylene Impact Copolymer Resin OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f.. |