Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1690 MPa | 245000 psi | 0.05 in/min test speed |
Ineos H53N-00 Polypropylene Homopolymer This is a high flow rate nucleated and lightly lubricated homopolymer polypropylene designed for high-speed injection molding of thin-walled parts requiring good stiffness and fast cycle times. Thi.. |