Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H53N-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H53N-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high flow rate nucleated and lightly lubricated homopolymer polypropylene designed for high-speed injection molding of thin-walled parts requiring good stiffness and fast cycle times. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsMedia packagingConsumer productsHousewaresThin-wall rigid packagingFood service productsBenefitsHigh flow rateFast cycle timesGood stiffnessVery good molding performance in thin-walled partsInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 53 g/10 min

@Load 2.16 kg,
Temperature 230 °C
53 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 41.3 MPa

@Temperature 23.0 °C
5990 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 33 %
33 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus, 1% Secant 1690 MPa
245000 psi
0.05 in/min test speed
Izod Impact, Notched 0.240 J/cm

@Temperature 23.0 °C
0.450 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution