Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1620 MPa | 235000 psi | 0.05 in/min; ASTM D790 |
Phillips 66 COPYLENE® CH005 Polypropylene, Homopolymer, Extrusion, Strapping COPYLENE® CH005 is a fractional melt flow polypropylene homopolymer resin available in pellet form.Information provided by Phillips 66. |
|||
Flexural Modulus, 1% Secant | 1620 MPa | 235000 psi | ASTM D790 |
Flint Hills P4G3B-146 Polypropylene Homopolymer Features: Nucleated and Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: general purposeInformation Provided by Flint Hills Resources |