Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1080 MPa | 156000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP7505KNE2 Polypropylene Homopolymer Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced .. |
|||
Flexural Modulus, 1% Secant | 1080 MPa | 156000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP8244E1 Polypropylene Homopolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Bala.. |