Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 896 MPa | 130000 psi | ASTM D790B |
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus, 1% Secant | 896 MPa | 130000 psi | ASTM D790B |
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus, 1% Secant | 896 MPa | 130000 psi | ASTM D790 |
ExxonMobil HDPE HPA 020 Wire & Cable High Density Polyethylene Resin Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer sh.. |
|||
Flexural Modulus, 1% Secant | 896 MPa | 130000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP9513 Polypropylene Homopolymer Product Description: A random copolymer resin designed for non-oriented film.Availability: North America Features:Controlled RheologyEthylene Oxide SterilizableUses: BagsCast FilmHeavy-duty BagsPac.. |