Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1170 MPa | 170000 psi | ASTM D790 |
Flint Hills P9G1Z-047 Polypropylene Features: Processing stability. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: Thick sheetingInformation Provided by Flint Hills Resources |
|||
Flexural Modulus, 1% Secant | 1170 MPa | 170000 psi | ASTM D790B |
ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |