Polymer Property : Tear Strength = 87.9 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 15.4 kN/m

@Temperature 23.0 °C
87.9 pli

@Temperature 73.4 °F
Die C; initial; infiltrated with flexseal (8-dip process)
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems
Thermoplastic elastomer material with rubber-like flexibility and functionality. For use with all selective laser sintering SLS® systems.ApplicationsAthletic footwear and equipmentGaskets, hoses an..