Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.4 kN/m @Temperature 23.0 °C |
87.9 pli @Temperature 73.4 °F |
Die C; initial; infiltrated with flexseal (8-dip process) |
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems Thermoplastic elastomer material with rubber-like flexibility and functionality. For use with all selective laser sintering SLS® systems.ApplicationsAthletic footwear and equipmentGaskets, hoses an.. |