Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 28.0 MPa @Temperature 23.0 °C |
4060 psi @Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |