Mechanical Properties Metric English Comments
Tensile Strength at Break 179 MPa

@Temperature -40.0 °C
26000 psi

@Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Rynite® 408 BK515 PET
Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info..