Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 179 MPa @Temperature -40.0 °C |
26000 psi @Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |