Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.9 MPa @Temperature 23.0 °C |
2020 psi @Temperature 73.4 °F |
Die C Across Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Tensile Strength at Break | 13.9 MPa @Treatment Temp. 25.0 °C, Time 252000 sec |
2020 psi @Treatment Temp. 77.0 °F, Time 70.0 hour |
Aged fuel C |
LG Chemical NBR 3250 High Acrylonitrile Polymer Description: NBR 3250 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3250 is a non staining, medi.. |