Polymer Property : Tensile Strength at Break = 13.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.9 MPa

@Temperature 23.0 °C
2020 psi

@Temperature 73.4 °F
Die C Across Flow 2 hr; ASTM D412
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tensile Strength at Break 13.9 MPa

@Treatment Temp. 25.0 °C,
Time 252000 sec
2020 psi

@Treatment Temp. 77.0 °F,
Time 70.0 hour
Aged fuel C
LG Chemical NBR 3250 High Acrylonitrile Polymer
Description: NBR 3250 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3250 is a non staining, medi..