Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.2 MPa @Time 86400 sec |
1910 psi @Time 24.0 hour |
Press Cure 10 Minutes @ 165°C (330°F) Ramp Post Cure in Air, Time Held at 300°C (572°F); ASTM D412 Die D Dumbbells |
3M Dyneon™ PFE 300Z Clear Perfluoroelastomer System Features and Benefits:Proprietary polymer and catalyst system enables the manufacture of optically clear finished partsProportionate polymer and catalyst package simplifies the mixing processLow ext.. |