Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 10400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.0 MPa

@Temperature 175 °C
10400 psi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Tensile Strength at Break 72.0 MPa

@Temperature 175 °C
10400 psi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Tensile Strength at Break 72.0 MPa

@Temperature 175 °C
10400 psi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Copyright © lookpolymers.com All Rights Reserved