Izod Impact, Notched (ISO) 9.20 kJ/m²

@Temperature -30.0 °C
4.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Polyram RamSter PF306G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram.