Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.20 kJ/m² @Temperature -30.0 °C |
4.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram RamSter PF306G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram. |